Materials (Basel, Switzerland) Apr 2024In this study, a series of Ti-5Cr-xNb alloys with varying Nb content (ranging from 1 to 40 wt.%) were investigated to assess their suitability as implant materials....
In this study, a series of Ti-5Cr-xNb alloys with varying Nb content (ranging from 1 to 40 wt.%) were investigated to assess their suitability as implant materials. Comprehensive analyses were conducted, including phase analysis, microscopy examination, mechanical testing, and corrosion resistance evaluation. The results revealed significant structural alterations attributed to Nb addition, notably suppressing the formation of the ω phase and transitioning from α' + β + ω to single β phase structures. Moreover, the incorporation of Nb markedly improved the alloys' plastic deformation ability and reduced their elastic modulus. In particular, the Ti-5Cr-25Nb alloy demonstrated high values in corrosion potential and polarization resistance, signifying exceptional corrosion resistance. This alloy also displayed high bending strength (approximately 1500 MPa), a low elastic modulus (approximately 80 GPa), and outstanding elastic recovery and plastic deformation capabilities. These aggregate outcomes indicate the promising potential of the β-phase Ti-5Cr-25Nb alloy for applications in orthopedic and dental implants.
PubMed: 38612179
DOI: 10.3390/ma17071667 -
Journal of Clinical Medicine Apr 2024Fiber-reinforced composites (FRCs) have been proposed as an alternative to traditional metal alloys for the realization of frameworks in full-arch implant-supported...
Fiber-reinforced composites (FRCs) have been proposed as an alternative to traditional metal alloys for the realization of frameworks in full-arch implant-supported prostheses. The aim of the present in vitro study was to evaluate the deflection under load of seven prostheses endowed with frameworks made of different materials, including different types of fiber-reinforced composites (FRCs). A master cast with four implant analogues in correspondence with the two lateral incisors and the two first molars was used to create full-arch fixed prostheses with the same shape and different materials. Prostheses were made of the following different materials (framework+veneering material): gold alloy+resin (Au+R), titanium+resin (Ti+R), FRC with multidirectional carbon fibers+resin (ICFRC+AR), FRC with unidirectional carbon fibers+composite (UCFRC+C), FRC with glass fibers+resin (GFRC+AR), FRC with glass fibers+composite (GFRC+C), and resin (R, fully acrylic prosthesis). Flexural tests were conducted using a Zwick/Roell Z 0.5 machine, and the deflection of the lower surface of the prosthesis was measured in order to obtain load/deflection graphs. Greater rigidity and less deflection were recorded for UCFRC+C and GFRC+C, followed by Ti+R and Au+R. The greatest deformations were observed for resin alone, ICFRC+R, and GFRC+R. The results were slightly different in the incisal region, probably due to the greater amount of veneering material in this area. When used to realize full-arch frameworks, Au and Ti allow for predictable mechanical behavior with gradual deformations with increasing load. UCFRC also demonstrated good outcomes and less deflection than ICFRCs when loaded. The GFRC full-arch framework may be a valid alternative, although it showed greater deflections. Further studies are needed in order to evaluate how different prosthesis designs and material thicknesses might affect the outcomes.
PubMed: 38610826
DOI: 10.3390/jcm13072060 -
The Journal of Prosthetic Dentistry Jul 2024The surface topography of metal substrate can affect its bond to porcelain. A neodynium-doped yttrium aluminum garnet (Nd:YAG) laser has been introduced to modify the...
STATEMENT OF PROBLEM
The surface topography of metal substrate can affect its bond to porcelain. A neodynium-doped yttrium aluminum garnet (Nd:YAG) laser has been introduced to modify the metal surface topography and improve porcelain bond strength. However, studies on the effect of laser etching on metal to porcelain bond strength are lacking.
PURPOSE
The purpose of this in vitro study was to determine the effect of Nd:YAG laser etching on the surface roughness and wettability of and the porcelain bond strength to cobalt chromium (Co-Cr) substrate fabricated by milling and direct metal laser sintering (DMLS).
MATERIAL AND METHODS
Thirty-two 0.5×3×25-mm Co-Cr specimens were fabricated by milling soft Co-Cr (M group) and DMLS Co-Cr metal powder (DML group). The surface topography of representative specimens from each study group was assessed under a scanning electron microscope (SEM) and an atomic force microscope (AFM). All specimens were assessed for surface roughness using a contact profilometer, and for wettability with a contact angle goniometer. Half of the specimens of each study group (n=8) were subjected to surface laser etching by using a Nd:YAG laser. The specimens subjected to etching were assessed again for surface topography and wettability. All specimens in both study groups were veneered with porcelain. The porcelain bond strength was tested with a 3-point bend test in a universal testing machine. The results were statistically analyzed with 2-way ANOVA test followed by the post hoc Tukey test for pairwise comparisons (α=.05).
RESULTS
After etching, the M group had a higher mean ±standard deviation Ra and Rz of 2.9 ±0.6 and 17.7 ±3.2 µm and significantly better wettability and bond strength of 79 ±6 and 52 ±13 MPa. In contrast, after etching, the DMLS group had a significantly lower Ra and Rz of 7.9 ±2.4 and 41.8 ±9.3 µm and significantly lower wettability and bond strength of 87 ±4 and 70 ±10 MPa. The DMLS group had a significantly higher roughness and bond strength than the M group before and after laser etching. The SEM and AFM showed different surface topography in the study groups.
CONCLUSIONS
The manufacturing process of Co-Cr substrate had a significant effect on surface characteristics and porcelain bond strength. Laser etching improved the surface topography and bond strength of milled Co-Cr but not of DMLS Co-Cr.
Topics: Chromium Alloys; Surface Properties; Dental Porcelain; Lasers, Solid-State; Dental Bonding; Microscopy, Electron, Scanning; Dental Etching; Wettability; Microscopy, Atomic Force; Materials Testing; Dental Stress Analysis; Humans; In Vitro Techniques
PubMed: 38609765
DOI: 10.1016/j.prosdent.2024.03.040 -
Nanomaterials (Basel, Switzerland) Mar 2024Titanium and its alloys are extensively applied in artificial tooth roots because of their excellent corrosion resistance, high specific strength, and low elastic...
Titanium and its alloys are extensively applied in artificial tooth roots because of their excellent corrosion resistance, high specific strength, and low elastic modulus. However, because of their biological inertness, their surface needs to be modified to improve the osteointegration of titanium implants. The preparation of biologically active calcium-phosphorus coatings on the surface of an implant is one effective method for enhancing the likelihood of bone integration. In this study, osteoinductive peptides were extracted from oyster shells by using acetic acid. Two peptide-containing hydroxyapatite (HA) composite coatings were then prepared: one coating was prepared by hydrothermally synthesizing an HA coating in the presence of peptides (HA/P/M), and the other coating was prepared by hydrothermally synthesizing HA and then immersing the hydrothermally synthesized HA in a peptide solution (HA/P/S). Characterization results indicated that the composite HA coatings containing oyster shell-based peptides were successfully prepared on the alkali-treated pure titanium surfaces. The HA/P/M and HA/P/S composite coatings were found to exhibit excellent hydrophilicity. Protein adsorption tests confirmed that the HA/P/M and HA/P/S coatings had an approximately 2.3 times higher concentration of adsorbed proteins than the pure HA coating.
PubMed: 38607112
DOI: 10.3390/nano14070577 -
The Journal of Adhesive Dentistry Jan 2024To investigate the influence of contamination and different cleaning methods on resin bonding to cobalt-chro- mium (CoCr) alloy disks.
PURPOSE
To investigate the influence of contamination and different cleaning methods on resin bonding to cobalt-chro- mium (CoCr) alloy disks.
MATERIALS AND METHODS
A total of 160 CoCr disks were divided into 3 groups. The first group (N = 64) was air abraded with alumina particles and contaminated with a silicone disclosing agent and saliva; the second group (N = 64) was air abraded but not contaminated; the third group (N = 32) was neither air abraded nor contaminated. The first two groups were di- vided into 4 subgroups (N = 16) according to the cleaning method: ultrasonic bath in 99% isopropanol, use of a cleaning suspension of zirconium oxide particles, use of a cleaning suspension based on 10-MDP salt, and treatment with atmo- spheric plasma. The third group was divided into 2 subgroups (N = 16): treatment with atmospheric plasma and no treat- ment. All CoCr specimens were bonded to plexiglas tubes filled with a bonding resin that contained phosphate monomer. Tensile bond strength (TBS) was examined by tensile testing after 3 and 150 days of water storage plus 37,500 thermal cy- cles (N = 8).
RESULTS
After contamination, TBS was significantly reduced after 150 days of water storage. Groups without air abrasion showed initially low TBS and debonded spontaneously after 150 days of water storage.
CONCLUSION
None of the cleaning methods was able to remove saliva and silicone disclosing agent on CoCr-alloy sur- faces. Surface activation by plasma treatment has no long-term effect on the bond strength.
Topics: Composite Resins; Resin Cements; Alloys; Air Abrasion, Dental; Dental Bonding; Surface Properties; Water; Tensile Strength; Silicones; Materials Testing; Zirconium; Dental Stress Analysis
PubMed: 38602286
DOI: 10.3290/j.jad.b5200039 -
Journal of the Mechanical Behavior of... Jun 2024Polyetheretherketone (PEEK) is considered as an alternative to metal material for removable partial denture (RPD). However, the retentive force is not strong as a metal...
PURPOSE
Polyetheretherketone (PEEK) is considered as an alternative to metal material for removable partial denture (RPD). However, the retentive force is not strong as a metal RPD. This study investigated the retention and fatigue performance of PEEK clasps with different proportions of clasp arm engaging the undercut to verify a new strategy to improve their clinical performance.
METHODS
Three groups (n = 10/group) of PEEK clasps with their terminal 1/3, 2/3 and the whole of retentive arms engaging the undercut were fabricated along with a group (n = 10) of conventional cobalt-chrome (CoCr) clasps as control group. Retentive forces were measured by universal testing machine initially and at an interval of 1500 cycles for a total of 15,000 fatigue cycles. The fatigue cycles were conducted by repeated insertion and removal of the clasp using fatigue testing machine. Each clasp was scanned by Trios3 scanner before and after fatigue test to obtain digital models. The deformation of the clasp was evaluated by root mean square (RMS) through aligning the two models in Geomagic wrap (2021). Scanning electron microscopy (SEM) and finite element analysis were carried out to observe the abrasion and the von Mises stress of the clasp arm. Kruskal-Wallis H test was used to compare the retentive forces and the RMSs of the studied groups followed by Bonferroni multiple comparisons.
RESULTS
The whole of PEEK clasp arm engaging the undercut provided higher mean retentive forces (7.99 ± 2.02 N) than other PEEK clasp groups (P < 0.001) and was closer to CoCr clasps (11.88 ± 2.05 N). The RMSs of PEEK clasps were lower than CoCr clasps (P < 0.05) while the differences among PEEK clasps were of no statistical significance (P > 0.05). SEM showed that evidences of surface abrasion were observed on the section that engaged the undercut for all groups of clasps. The stress concentration mainly occurred on the initial part of the retentive arm. The maximum von Mises stress of each group was below the compressive strength of PEEK.
CONCLUSIONS
Proportions of PEEK clasp arm engaging the undercut positively influenced the retentive force and the fatigue resistance of PEEK clasps was superior than CoCr clasps. It is a feasible method to improve the retention of PEEK clasps by increasing the proportion of clasp arm engaging the undercut. Clinical trials are needed to further verify this innovation.
Topics: Denture Retention; Polyethylene Glycols; Polymers; Ketones; Chromium Alloys; Denture, Partial, Removable; Dental Stress Analysis; Dental Clasps; Benzophenones
PubMed: 38598917
DOI: 10.1016/j.jmbbm.2024.106539 -
Journal of Pharmacy & Bioallied Sciences Feb 2024Surface roughness of the crowns is dependent on the pattern material used for the making as well as the procedure of investing. The study was aimed to examine the impact...
INTRODUCTION
Surface roughness of the crowns is dependent on the pattern material used for the making as well as the procedure of investing. The study was aimed to examine the impact of various pattern materials and investment procedures on the surface roughness of nickel-chromium alloy raw castings.
MATERIALS AND METHODS
An study was piloted at a tertiary care hospital. Eighty samples of inlay wax and pattern resin were divided equally. They were invested in phosphate-bonded investment material and kept under normal atmospheric pressure as well as invested under a pressure of 3 bars. The surface roughness was calculated with a Profilometer. The values obtained were compared using statistical tools keeping < 0.05 as significant.
RESULTS
Lowest surface roughness was seen for the wax pattern invested under positive pressure. While the highest was seen for the resin patterns invested at room pressure. A significant variance between the wax 1 and wax 2 ( < 0.01); as well as between the wax 2 vs. Resin 2 specimens ( < 0.01) was noted.
CONCLUSIONS
Wax patterns can be suggested as the material and method of choice because they showed the least amount of surface roughness when placed under pressure. Resin patterns when invested under pressure can also be suggested as an alternate as they also exhibited similar surface roughness as that of the wax.
PubMed: 38595557
DOI: 10.4103/jpbs.jpbs_445_23 -
Journal of Pharmacy & Bioallied Sciences Feb 2024The esthetic during the various orthodontic treatments has led to the invention of the brackets. When different ceramic brackets and archwires are used, the different...
INTRODUCTION
The esthetic during the various orthodontic treatments has led to the invention of the brackets. When different ceramic brackets and archwires are used, the different frictional forces may result in the different outputs. Hence, in the present study, we evaluated and compared the frictional resistance between eight standard monocrystalline ceramic bracket models and each of the archwires of four different alloys.
MATERIALS AND METHODS
Frictional force was tested using Instron testing machine, , for eight types of monocrystalline ceramic bracket, and four types of archwires beta-titanium, NiTi, copper-nickel-titanium, and stainless steel statistical analysis were done using various tools, and significance value of <0.05 was considered.
RESULTS
Ormco and AO (Radiance) monocrystalline ceramic brackets created lesser frictional resistance than other monocrystalline ceramic brackets. Stainless steel archwire generates lesser static friction. Beta-titanium archwire created higher static friction. A 0.017 × 0.025 inch stainless steel archwire generates lesser static friction to 0.019 × 0.025 inch TMA.
CONCLUSION
It can be concluded that Ormco and AO (Radiance) monocrystalline ceramic brackets, with stainless steel archwires and of size 0.017 × 0.025 inch, can generate better forces when used for the orthodontic tooth movements.
PubMed: 38595439
DOI: 10.4103/jpbs.jpbs_572_23 -
Journal of Prosthodontics : Official... Apr 2024Bioceramic coatings have been shown to promote bone repair, which aids in the early integration of implants. This study aimed to evaluate the influence of air abrasion...
PURPOSE
Bioceramic coatings have been shown to promote bone repair, which aids in the early integration of implants. This study aimed to evaluate the influence of air abrasion with a bioceramic abrasive on the surface characteristics of different implant materials and surfaces. The dissolution of the applied treatment from the surfaces over 3 weeks was also assessed.
MATERIALS AND METHODS
Discs of three alloys used for dental implants were studied and compared: two types of commercially pure titanium (CpTi)/ (CpTi SLActive) and titanium-zirconia (TiZr). The tested surfaces were: CpTi control (CpC), sandblasted (SB), sandblasted and acid-etched (SBE), and CpTi SLActive®, (TiZr) Roxolid®. Three discs from each group underwent air abrasion with apatite bioceramic powders, 95% hydroxyapatite (HA)/5% calcium oxide (CaO), and 90% hydroxyapatite (HA)/10% calcium oxide (CaO). The treated discs were surface characterized by optical profilometry to obtain surface roughness, scanning electron microscopy (SEM), and energy dispersive X-ray spectroscopy (EDS) to compare element weight percentages of titanium, calcium, and phosphate. Dissolution was assessed using inductively coupled plasma optic emission spectrometry (ICP-OES).
RESULTS
Bioceramic powders were deposited on all tested surfaces leading to changes in surface characteristics. The only statistically significant differences between the material groups for surface roughness were found with 95% HA/5% CaO powder in the Sp and Rp parameters (p = 0.03 and 0.04, respectively). There were no significant differences in the Ca and P wt% between all groups and powders 95% HA/5% CaO and 90% HA/10% CaO (p = 0.14, 0.18, and p = 0.15, 0.12, respectively). A non-uniform dispersion of the treatment on the surface layer was visible on all treated surfaces. The bioceramic powder continued to dissolute from the tested surfaces for 3 weeks.
CONCLUSION
Bioceramic abrasion modifies implant surface characteristics, although the change in surface characteristics resulting from such treatment was not influenced by the implant material or surface treatment. Air abrasion with hydroxyapatite and calcium oxide bioceramics leaves powder deposits on the treated implant surfaces that could potentially influence the healing of implants affected by peri-implantitis.
PubMed: 38594924
DOI: 10.1111/jopr.13857 -
Environmental Geochemistry and Health Apr 2024Advancement in bioinspired alloy nanomaterials has a crucial impact on fuel cell applications. Here, we report the synthesis of PtPd alloy nanoclusters via the...
Advancement in bioinspired alloy nanomaterials has a crucial impact on fuel cell applications. Here, we report the synthesis of PtPd alloy nanoclusters via the hydrothermal method using Piper longum extract, representing a novel and environmentally friendly approach. Physicochemical characteristics of the synthesized nanoclusters were investigated using various instrumentation techniques, including X-ray photoelectron spectroscopy, X-ray diffraction, and High-Resolution Transmission electron microscopy. The electrocatalytic activity of the biogenic PtPd nanoclusters towards the oxidation of formic acid and methanol was evaluated chronoamperometry and cyclic voltammetry studies. The surface area of the electrocatalyst was determined to be 36.6 mg by Electrochemical Surface Area (ECSA) analysis. The biologically inspired PtPd alloy nanoclusters exhibited significantly higher electrocatalytic activity compared to commercial Pt/C, with specific current responses of 0.24 mA cm and 0.17 mA cm at synthesis temperatures of 180 °C and 200 °C, respectively, representing approximately four times higher oxidation current after 120 min. This innovative synthesis approach offers a promising pathway for the development of PtPd alloy nanoclusters with enhanced electrocatalytic activity, thereby advancing fuel cell technology towards a sustainable energy solution.
Topics: Methanol; Alloys; Piper; Plant Extracts; Formates
PubMed: 38592578
DOI: 10.1007/s10653-024-01953-0